Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 9700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 66.9 MPa
9700 psi
ASTM D790
Multibase Nylex™ 2185 HFX Natural Polyamide + PP
Forms: PelletsProcessing Methods:Injection moldingFeatures:Tensile Strength, HighInformation provided by Multibase
Flexural Strength 66.9 MPa
9700 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid)
Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne
Flexural Strength 66.9 MPa
9700 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 66.9 MPa
9700 psi
ASTM D790
PolyOne Geon™ Vinyl Rigid Molding M5705 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Flexural Strength 66.9 MPa
9700 psi
Poco Graphite EDM-1 EDM Graphite
Applications:Fabricating electrodes with good detail Low wear electrodes High detail roughing electrodesMolds and dies
Flexural Strength 66.9 MPa
9700 psi
ASTM D790
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa..
Flexural Strength 66.9 MPa
9700 psi
ASTM D790
PolyOne Geon™ HTX Ultra LA426 Tan 3725 Polyvinyl Chloride Alloy (PVC Alloy)
Optimum for Black and Darker Colors between 50 and 70 L value. Also suitable for colors above 70 L value.Recommend drying material for a minimum of 2 hours at 160 degrees Farenheit. Physical propert..
Flexural Strength 66.9 MPa

@Temperature 100 °C
9700 psi

@Temperature 212 °F
ISO 178
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
Flexural Strength 66.9 MPa

@Temperature 100 °C
9700 psi

@Temperature 212 °F
2; ISO 178
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
Flexural Strength 66.9 MPa
9700 psi
ASTM D638
Amco Amalloy® B1172 Polymer Alloy
Amco Amalloy B1172 is a proprietary copolymer with exceptional clarity and enhanced impact strength.Impact modified, very clear, moderate flow.Information provided by Amco Plastic Materials.
Flexural Strength 66.9 MPa
9700 psi
3M Scotchkote™ HTX 517 Epoxy HT Lining
Scotchkote Epoxy HT Lining HTX 517 has been specifically developed as a 100% solids epoxy coating for resurfacing and lining equipment operating at high temperatures.Product Features:Combines good a..
Flexural Strength 66.9 MPa
9700 psi
ASTM D790
PolyOne Edgetek® ATH-15GF/000 Acetal-Homopolymer, Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.