Mechanical Properties Metric English Comments
Graves Tear Strength 33.5 kN/m

@Temperature 23.9 °C
191 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys DuraGrip™ DGR 6080 NC/BK Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6080NC/BK are designed to be a general purpose Thermoplastic Elastomers (TPE) that are easy to use in injection molding and extrusion processes. DGR 6080NC/BK have excellent soft touc..