Graves Tear Strength 210 kN/m
1200 pli
Die C; ASTM D624
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection MoldingAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Graves Tear Strength 210 kN/m
1200 pli
Die C; ASTM D624
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Type: Estane® ETE 70DT3 is an aromatic polyether-based thermoplastic polyurethane (TPU).Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, hig..