Polymer Property : Graves Tear Strength = 218 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 38.2 kN/m
218 pli
TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Trefsin® 3101-85 W305 Thermoplastic Rubber  (discontinued **)
A black thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing tec..
Graves Tear Strength 38.2 kN/m
218 pli
TPE-0056 (ASTM D 624)
Advanced Elastomer Systems Trefsin® 3201-85 W305 Thermoplastic Rubber  (discontinued **)
A natural thermoplastic elastomer with excellent permeation resistance to water, air and other gases. It can be processed using injection molding, extrusion, blow molding or other melt processing t..