Polymer Property : Graves Tear Strength = 38.6 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 38.6 kN/m

@Temperature 23.9 °C
220 pli

@Temperature 75.0 °F
Die C; ASTM D624; DIN 53507
Advanced Polymer Alloys Alcryn® 2165 NC Melt Processable Rubber
Alcryn 2100 Series melt-processable rubber (MPR) offer a broader range of bonding to rigid substrates while maintaining all the excellent performance features of traditional Alcryn. The 2100 grades..
Graves Tear Strength 38.6 kN/m

@Temperature 23.9 °C
220 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 4670 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 38.6 kN/m

@Temperature 23.9 °C
220 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 4670 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 38.6 kN/m

@Temperature 23.9 °C
220 pli

@Temperature 75.0 °F
Die C; ASTM D624; DIN 53507
Advanced Polymer Alloys DURACRYN 8070 NC Thermoplastic Rubber
Information provided by Advanced Polymer Alloys