Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 75.3 kN/m | 430 pli | TD; ASTM D1004 |
DuPont Nucrel® 31001 Ethylene-Acrylic Acid Copolymer Resin for Blown and Cast Film 9.5 wt% Acrylic Acid.Nucrel® 31001 is an ethylene-acrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins.F.. |