Polymer Property : Graves Tear Strength = 480 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 84.1 kN/m
480 pli
Die C; ASTM D624
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane
Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E..