Compressive Yield Strength 0.0950 MPa
13.8 psi
40% Compression, ASTM D3574-C
Covestro Bayfill® 361 Polyurethane Semi-Rigid Foam, Conventional Catalyst, Open Pour, MDI-based 2-Component Liquid System
Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.