Mechanical Properties Metric English Comments
Compressive Yield Strength 0.00172 - 0.00931 MPa

@Strain 25.0 %
0.250 - 1.35 psi

@Strain 25.0 %
0.2"/min. strain rate
Rogers Corporation Poron® 4790-92-09 Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
Compressive Yield Strength 0.00172 - 0.0172 MPa

@Strain 25.0 %
0.250 - 2.50 psi

@Strain 25.0 %
0.2"/min. strain rate
Rogers Corporation Poron® 4790-92-12 P Series Urethane Foam, Extra Soft, Slow Rebound, PET Film Reinforced
Extra soft, slow rebound with a very low closure force. Standard available thickness range from 0.021" to 0.500" (0.53 mm to 12.7 mm).Features and Benefits of PORON Products: Excellent compression ..
Compressive Yield Strength 0.00172 - 48.0 MPa
0.250 - 6960 psi
Average value: 2.16 MPa Grade Count:134
Overview of materials for Thermoset Polyurethane Foam, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu..