Mechanical Properties Metric English Comments
Compressive Yield Strength 0.00731 MPa

@Strain 25.0 %
1.06 psi

@Strain 25.0 %
0.2"/min. strain rate
Rogers Corporation Poron® ThinStik ShockSeal™ 79-09021 Self-Adhesive Urethane Foam
PORON® ThinStik™ materials utilize an acrylic pressure sensitive adhesive manufactured to Roger's specifications. This adhesive provides reliable bonding to a wide variety of substrates, exhibits..