Mechanical Properties Metric English Comments
Compressive Yield Strength 793 MPa
115000 psi
longitudinal
ATI Allegheny Ludlum Stainless Steel Type 301, Full Hard (UNS S30100)
Allegheny Ludlum Type 301 is a high strength grade of steel available in six conditions or tempers, its resistance to atmosphere corrosion and its bright, attractive surface make it an excellent cho..