Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 838 MPa | 122000 psi | 0° Fiber Direction; ASTM D3410 |
Saint-Gobain Quartzel® Fiber/Cyanate Ester Resin Unidirectional Composite Fiber: Quartzel® Silica Roving C9 667 QS16 (33). Resin: YLA RS-3C.Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous,.. |