Polymer Property : Compressive Yield Strength = 130.0 MPa
Polymer Property :
Compressive Yield Strength =
130.0 MPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Compressive Yield Strength
130.0
MPa
18850
psi
ASTM D695
Devcon High-Performance Backing Compound Epoxy
Abrasion-Resistant SystemData provided by Ellsworth Adhesives.