Mechanical Properties Metric English Comments
Compressive Yield Strength 98.6 MPa
14300 psi
ASTM D695
Fibre Glast 1101 High-Strength General Purpose Epoxy Adhesive
Description:#1101 is a light grayish-tan two part epoxy adhesive that was developed especially for difficult bonding problems involving similar or dissimilar materials. #1101 provides excellent adhe..