Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 144 - 169 MPa | 20800 - 24500 psi | Average value: 160 MPa Grade Count:6 |
Overview of materials for Polyethylene Terephthalate (PET), Recycled, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Recycled, Glass Reinforced". Each property range of values reported is.. |