Compressive Yield Strength 120 - 1000 MPa
17400 - 145000 psi
Average value: 292 MPa Grade Count:57
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..