Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 146 MPa | 21200 psi | DIN EN ISO 604 |
Wolf Kunststoff ZEDEX® ZX-324V11T A3L PEEK Polymer, Reinforced Main Charactistics: Stress resistant; High impact strength at 196 ° C Applications: Shipbuilding; Chemical Engineering; Automitve Technology; Machine ToolsInformation provided by Zedex |
|||
Compressive Yield Strength | 146 MPa | 21200 psi | |
Hexcel® HexPly® M36 180°C (350°F) Curing Epoxy Matrix HexPly® M36 is a high performance 180ºC cure matrix developed for aerospace and industrial markets. It can be used in a variety of production techniques (Resin Film Infusion (RFI), prepreg and sem.. |