Polymer Property : Compressive Yield Strength = 151 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 1.04 MPa
151 psi
at 10% Compression, Parallel to thickness
Zircar Ceramics SALI-2 Alumina Insulation
SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics.