Polymer Property : Compressive Yield Strength = 155 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 60.0 - 155 MPa

@Temperature 120 - 200 °C
8700 - 22500 psi

@Temperature 248 - 392 °F
Average value: 93.3 MPa Grade Count:2
Overview of materials for Polyetheretherketone, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values..