Compressive Yield Strength 157 - 215 MPa
22800 - 31200 psi
Average value: 189 MPa Grade Count:10
Overview of materials for Phenolic, Resole, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Wood Filled". Each property range of values reported is minimum and maximum values of ..
Compressive Yield Strength 157 MPa
22800 psi
Haveg 41N Phenolic; Silicate Reinforced Ablative Material
A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers converted to a permanent thermoset state under heat and pressure. It is designed for abla..