Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 161.8 MPa | 23470 psi | ASTM D695 |
Plenco 51240 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P.. |