Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 112.38 MPa | 16299 psi | |
Abatron AboCast 50-3/AboCure 50-12 Epoxy Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months. |