Mechanical Properties Metric English Comments
Compressive Yield Strength 17.2 MPa
2500 psi
TM R050-38
Resinlab® EP1287 Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1287 is a two part filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-extinguishin..
Compressive Yield Strength 17.2 MPa
2500 psi
TM R050-38
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam
Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti..
Compressive Yield Strength 17.2 MPa
2490 psi
at 10% deflection, parallel to thickness
Zircar Refractory Composites RS-A3 Refractory Sheet
This product is made from Type RS-A Moldable. Type RS-A was developed as an asbestos board replacement for induction coil liners and molten metal transport, and contains no asbestos. Refractory Shee..
Compressive Yield Strength 17.2 MPa
2500 psi
TM R050-38
Resinlab® EP1305LV Black Epoxy Casting Resin
Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..
Compressive Yield Strength 17.2 MPa
2500 psi
TM R050-38
Resinlab® EP1305LV Clear Epoxy Casting Resin
Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c..