Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 1720 MPa | 249000 psi | |
Cytec Thornel® P-650/35 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |
|||
Compressive Yield Strength | 1720 MPa | 249000 psi | |
Cytec Thornel® P-650/42 Carbon Fiber/Epoxy Advanced Composite System Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco .. |