Mechanical Properties Metric English Comments
Compressive Yield Strength 183 - 226 MPa
26600 - 32800 psi
Average value: 206 MPa Grade Count:15
Overview of materials for Phenolic; Unreinforced; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic; Unreinforced; Molded". Each property range of values reported is minimum and maximum values of..