Compressive Yield Strength 190 MPa
27600 psi
ASTM D695
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, at 50% RH  (dis
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre..
Compressive Yield Strength 190 MPa
27600 psi
ASTM D695
Albis Plastics Tedur® L V 9404-1 PPS, 30% Carbon Fiber  (discontinued **)
High Electrical and Thermal Conductivity, Long-term Anti-static Properties. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fan Blades, Brake Sleeves, Model Constructi..