Compressive Yield Strength 1350 MPa
196000 psi
0.2%, hardened to 50 HRC
Bohler-Uddeholm AISI A2 Cold Work Tool Steel
Description: AISI A2 is an air- or oil hardening chromiummolybdenum-vanadium alloyed tool steel characterized byAISI A2 is characterized by: Good machinability High stability after hardening High c..
Compressive Yield Strength 1350 MPa
196000 psi
0.2%, hardened to 50 HRC
Bohler-Uddeholm O1 Cold Work Tool Steel
Manganese-chromium-tungsten alloyed steelA general purpose oil hardening tool steel suitable for back up and punch holder plates. Features of this grade include a good combination of high surface ha..