Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 4.14 - 1360 MPa | 600 - 197000 psi | Average value: 268 MPa Grade Count:38 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |