Compressive Yield Strength 2.91 MPa
422 psi
FiberNide Nickel Aluminide Foam Atomic 22% Aluminum
Description: This Nickel aluminide foam has excellent high temperature strength, oxidation resistance, and conductivity. This unique combination of properties makes this foam particularly suitable f..