Mechanical Properties Metric English Comments
Compressive Yield Strength 11.0 - 14.0 MPa
1600 - 2030 psi
1% deformation; ISO 604
Arkema Group VOLTALEF® 300 HD PCTFE
VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group
Compressive Yield Strength 11.0 - 14.0 MPa
1600 - 2030 psi
1% deformation; ISO 604
Arkema Group VOLTALEF® 302 PCTFE
VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group
Compressive Yield Strength 4.00 - 14.0 MPa
580 - 2030 psi
Average value: 10.0 MPa Grade Count:3
Overview of materials for Polypropylene, Extrusion Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of..