Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 96.5 - 148 MPa | 14000 - 21500 psi | Average value: 114 MPa Grade Count:3 |
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a.. |
|||
Compressive Yield Strength | 33.0 - 148 MPa | 4790 - 21500 psi | Average value: 87.0 MPa Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum .. |