Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 15.0 MPa | 2180 psi | at 2% nominal strain; ISO 604 |
Quadrant EPP Cesticolor™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Compressive Yield Strength | 15.0 MPa | 2180 psi | at 2% nominal strain; ISO 604 |
Quadrant EPP Cestilene™ HD 500 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |
|||
Compressive Yield Strength | 15.0 MPa | 2180 psi | at 5% nominal strain; ISO 604 |
Quadrant EPP Cestlite™ ASTL Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |