Polymer Property : Compressive Yield Strength = 2200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength >= 15.2 MPa
>= 2200 psi
Bare, min
Hexcel® HexWeb® CFC™-20-1/8-11.0 Composite Flooring Honeycomb Core
Hexweb CFC™-20 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes and, after expanding to the hexagonal confiation, the block is dipp..
Compressive Yield Strength >= 15.2 MPa
>= 2200 psi
Stabilized, min
Hexcel® HexWeb® CR III 1/8-5052-.003 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..
Compressive Yield Strength >= 15.2 MPa
>= 2200 psi
Stabilized, min
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0037 Phosphoric Acid Anodized Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa..
Compressive Yield Strength 15.2 MPa
2200 psi
Aptek DI-STRATE 1503 Microwave/RF Foam Substrate
DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: MicrowaveInformation provided by Aptek Labo..