Mechanical Properties Metric English Comments
Compressive Yield Strength 15.5 MPa

@Strain 10.0 %
2250 psi

@Strain 10.0 %
Saint-Gobain Rulon® II Bearing/Seal PTFE
An injection moldable bearing material that possesses excellent chemical and wear resistance. Rulon II is available in injection molded finished parts only. Excellent friction and wear properties al..
Compressive Yield Strength 15.5 MPa
2250 psi
Stabilized, typ, preliminary
Hexcel® HexWeb® CR III 1/8-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb
Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR..