Compressive Yield Strength 2290 MPa
332000 psi
0.2%, hardness of 60 HRC, tempered at 977°F 2 + 2h.
Bohler-Uddeholm UDDEHOLM VANADIS 6 Cold Work Tool Steel
Description: Chromium-molybdenum-vanadium alloyed PM steel. Toolmaking with highly alloyed tool steel means that machining and heat treatment have to be considered more than with lower alloyed grade..