Polymer Property : Compressive Yield Strength = 23100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 159 - 314 MPa
23100 - 45500 psi
Average value: 213 MPa Grade Count:7
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Compressive Yield Strength 159.3 MPa
23100 psi
ASTM D695
Plenco 50240 PET, Pellet, Injection Molded, Natural Color  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..
Compressive Yield Strength 159 MPa
23100 psi
10% Strain; EN ISO 604
Ensinger TECASINT™ 2021 Polyimide, 15% Graphite (PI)
TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications...
Compressive Yield Strength 159 MPa
23100 psi
ASTM D695
Adell BL-18 Nylon 6, 40% Glass Reinforced; Mineral Filled
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 159 MPa
23100 psi
ASTM D695
Adell BL-38 Nylon 6, 40% Glass Reinforced; Mineral Filled
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 159 MPa
23100 psi
ASTM D695
Adell BW-37 Nylon 6, 35% Glass Reinforced; Superior Finish
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 159 MPa
23100 psi
ASTM D695
Adell AJ-17 Nylon 66, 35% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 159 MPa
23100 psi
ASTM D695
Adell AJ-37 Nylon 66, 35% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
Compressive Yield Strength 159 MPa
23100 psi
ASTM D695
Adell BW-17 Nylon 6, 35% Glass Reinforced; Superior Finish
Data provided by Adell Plastics, Inc.