Polymer Property : Compressive Yield Strength = 23550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 162.4 MPa
23550 psi
ASTM D695
Plenco 7527 Phenolic, Nodular, Injection Molded  (discontinued **)
Single-Stage Phenolic. PLENCO 07527 is a flock cotton and mineral filled resole phenolic molding compound.Information supplied by Plenco