Polymer Property : Compressive Yield Strength = 23900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 68.9 - 165 MPa
10000 - 23900 psi
Average value: 114 MPa Grade Count:20
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..