Mechanical Properties Metric English Comments
Compressive Yield Strength 25.6 MPa
3710 psi
at 10% deflection, parallel to thickness
Zircar Refractory Composites RS-99W Refractory Sheet
Type RS-99W boards can be moistened with water and molded into any desired shape. After low temperature bake-out of 300°C (570°F) boards are unaffected by moisture.Information provided by ZIRCAR R..