Mechanical Properties Metric English Comments
Compressive Yield Strength 185.1 MPa
26850 psi
ASTM D695
Plenco 50030 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50030 is an engineering grade glass reinforced polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in white, natural, and black.Information sup..