Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 29.0 MPa | 4210 psi | ASTM D695 |
Protective Coating PC-7® Epoxy Paste PC-7® is a tough job Epoxy formulation developed for maximum bonding power. Components A (grey) and B (black), when mixed, react to form a bond of good strength. PC-7® formulation provides exten.. |
|||
Compressive Yield Strength | 29.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
4210 psi @Strain 1.00 %, Time 1000 hour |
ASTM D695 |
Manifattura Cattaneo VESPEL® SP21 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Compressive Yield Strength | 29.0 - 147 MPa | 4210 - 21300 psi | Average value: 66.6 MPa Grade Count:12 |
Overview of materials for Nylon 6, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Heat Stabilized". Each property range of values reported is minimum and maximum values of appro.. |
|||
Compressive Yield Strength | 29.0 - 34.5 MPa | 4200 - 5000 psi | Average value: 32.1 MPa Grade Count:4 |
Overview of materials for Polypropylene Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o.. |