Compressive Yield Strength 80.0 - 320 MPa
11600 - 46400 psi
Average value: 146 MPa Grade Count:29
Overview of materials for Phenolic, Novolac, Fabric Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Fabric Filled". Each property range of values reported is minimum and maximum values ..