Compressive Yield Strength 2.50 MPa
363 psi
Stabilised
Hexcel® HexWeb® CRF-1/4-ACG-.002-3.4 Chromate free ACG® Honeycomb
Hexweb CRF is a hexagonal cell aluminum honeycomb material used principally as a shear carrying core in light weight adhesively bonded sandwich structures, and suitable for a wide range of other app..