Polymer Property : Compressive Yield Strength = 37.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 37.9 MPa
5500 psi
TM R050-38
Resinlab® EP1056LV Black Urethane Modified Epoxy Casting Resin
Resinlab™ EP1056LV Black is a two part urethane modified epoxy casting resin designed to give good adhesion to metals and PVC. It has good wetting to most surfaces and is free-flowing to penetrate ..