Polymer Property : Compressive Yield Strength = 38900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 70.0 - 268 MPa
10200 - 38900 psi
Average value: 160 MPa Grade Count:15
Overview of materials for Polyimide, Graphite Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Graphite Filled". Each property range of values reported is minimum and maximum values of app..