Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 4.50 MPa @Strain 1.00 % |
653 psi @Strain 1.00 % |
dry; ISO 604 |
Murtfeldt Murflor® Polytetrafluoroethylene Murflor® materials are suited to use in applications that require an excellent resistance to chemicals and heating steam. Murflor®’s working range starts at -200°C and can extend to +260°C with.. |
|||
Compressive Yield Strength | 4.50 MPa | 653 psi | at 1% nominal strain; ISO 604 |
Quadrant EPP Cestilene™ HD 1000 Polyethylene Data provided by Quadrant Engineering Plastic Products for polymers in their European product line. |