Polymer Property : Compressive Yield Strength = 4.50 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0310 MPa
4.50 psi
at 25% deflection; ASTM D1056
Rogers Corporation Bisco™ HT-870 Cellular Silicone Foam
Gasketing and sealing rating is JMLU-2 (Listed) per UL 157. No UV degradation per SAE J-1960. Ozone effect rating is 0 (no cracks) per ASTM D-1171. No staining per ASTM D-925(A). Passes AMS-3568..