Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 4.62 MPa | 670 psi | Stabilized, typ |
Hexcel® HexWeb® CR III 3/16-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Yield Strength | 4.62 MPa | 670 psi | Bare, typ |
Hexcel® HexWeb® HRH-10/F50 - 5.0 Nonmetallic Flex-Core Honeycomb Designation: Material/Cell Size (cells per lineal foot in W direction)-DensityHexcel manufactures two types of nonmetallic reinforced plastic HexWeb Flex-Core: HexWeb HRP - Fiberglasses cloth reinfo.. |
|||
Compressive Yield Strength | 4.62 MPa | 670 psi | Stabilized |
Hexcel® HexWeb® HRH-36 - 1/8 - 4.5 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Compressive Yield Strength | >= 4.62 MPa | >= 670 psi | Stabilized, min |
Hexcel® HexWeb® HRP/OX - 1/4 - 5.5 Fiberglass/Phenolic Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb HRP is a glass fabric reinforced honeycomb in which a heat-resistant phenolic resin is used both for initial and final impregnations. This prod.. |
|||
Compressive Yield Strength | 4.62 MPa | 670 psi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 3/16-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |