Polymer Property : Compressive Yield Strength = 40.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.104 - 0.276 MPa
15.1 - 40.0 psi
at 25% deflection; 0.2"/min strain rate
Rogers Corporation Poron® 4701-40-30 Cellular Urethane Foam
Information on this material is preliminary.Standard color is black (04); others are available. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F).General Poron® information: Poron® fo..