Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | >= 0.300 MPa | >= 43.5 psi | ASTM C365 |
Parabeam Industrie Paraglass 22 3D Glass Fabric Parabeam® 3D Glass Fabric is a fabric woven out of a 100% E-glass yarn and consists of two decklayers bonded together by vertical piles in a sandwich structure. These piles are woven into the deckl.. |
|||
Compressive Yield Strength | 0.300 MPa | 43.5 psi | 50% strain; ASTM D575 Method A |
Sorbothane Polyurethane Damping Material, 30 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m.. |
|||
Compressive Yield Strength | 0.300 - 67.6 MPa | 43.5 - 9800 psi | Average value: 17.4 MPa Grade Count:4 |
Overview of materials for Thermoset Polyurethane, Elastomer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Elastomer, Unreinforced". Each property range of values reported is minimum and .. |